Steel Rolling
1003-9996
2011 Issue 3
Forum on Products Development
LI Shi-jun
..............
page:1-7,37
Influence of Coiling Technology on Microstructure and Property of New Cold Rolled Non-oriented Electrical Steel
HU Guan-qiao;ZENG Yan-ping;WANG Li-jun
..............
page:18-20
xin xi dong tai
..............
page:17,26,30,33,42,58,69,72-76
The Design Characteristics of Continuous Hot-dip Galvanizing Line Developed by Baosteel
LI Jia;DING Yong-sheng;WANG Wen-hao
..............
page:34-37
Improvement of decoiling Equipment of Hot Coiling-box on 1422mm Hot Strip Line
SHI Lang-guo
..............
page:59-61
Study on Anti-corrosion Properties of Tannic Acid-H2 TiF6 Coating
XU Zhe-feng
..............
page:24-26
Effects of Carbon Equivalent on Microstructure and Properties of C-Mn Hot Rolled Dual-phase Steel
DONG Rui-feng;LI De-gang;YAN Bo;WANG Guo-dong
..............
page:11-13
Design and Application of Cooling Control System of Hot Rolled Strip
LIU Wei-wei;LI Hai-jun;WANG Zhao-dong;WANG Guo-dong
..............
page:47-50
Development of Five-strands Splitting Rolling Technology for Φ10mm Ribbed Bar
ZHAO Yan-peng;WU Yong;ZHANG Zhong-feng;LI Xi-bao
..............
page:64-67
Improvement on Straightening Process of Head End of the Long Rail
TAO Gong-ming;CHEN Chong-mu;LI Chun-ping
..............
page:27-30
Deduction and Application of New Spread Formulas for Plate Rolling
JIANG Ming-cai;ZHU Zhao-shun;SHENG Xi-gang;YANG Wen-bo
..............
page:14-17
Analyses on the Roller Elastic Deformation of 4-high CVC Mill
LIU Ai-min;LIU Guang-ming
..............
page:21-23
Design and Reformation of Short Length Workshop for Both Bar and High Speed Stainless Steel Production Lines
ZHONG Ting-zhen;ZHAI Shen-an;ZHONG Jian-yu;DONGShu-tong
..............
page:40-42
Shape Stability Control of 6mm Plate by Medium Plate Mill
CAO Kai-chen;HAO Xiao-qiang;WANG Shao-song;BAI Li
..............
page:51-53
Reformation of Horizontal Loop on 1250mm 8-high Five Tandem Mill
WANG Xing-wu;CHENG Ji-min;LI Shi-hua;ZHANG Jin
..............
page:38-40
Cause Analysis of Cracking of TQ295A Tank Steel by Press Forming
MENG Gang;HAO Xiao-qiang;WANG Xin;CAO Kai-chen
..............
page:62-64
Improvement on Loading Device of Skirt-plated Cooling Bed
HAN Xin-sheng;GAO Hong-chuan;MA Shu-long;WANG Huan-sheng;WANG Jing-yi
..............
page:68-69
Industrial Trial of HRBF400 Fine Grain Concrete Bar in Coil
CHEN Li-yong;LI Xiao-guang;GAO Lei;DING Da-wei;CHAI Jian-ming
..............
page:31-33
New Advance in Galvanizability and Internal Oxide Model of Advanced High-strength Steel
CUI Qing-ling;LI Jian-ping;ZHANG Xiao-ming
..............
page:43-46,53
Development of High Pressure and Low Flow Descaling System Used in Steckel Mill at Nanjing Iron & Steel Co., Ltd.
XIE Rui-chang;DANG Jun
..............
page:56-58
Technical Reformation of Reducing Annealing Furnace Used in Hot-dip Galvanizing Line at Jinan Iron & Steel Co., Ltd.
LU Qing-xiang;GAO Feng
..............
page:70-72
Measures of Reducing Width Deviation of Hot Rolled Medium-wide Strip
WANG Si-hai;BAO Jian-hua;YU Xiao-bo
..............
page:54-56
Development and Application of Direct Quenching Process of Steckel Mill Laminar Cooling System
HE Chun-yu;YU Wei;LIU Li-hua;YIN Yu-qun;TANG Yun-zhang;WANG Dao-yuan
..............
page:8-10